TIALCN, PVD Coating

Technical Specification
  Material : Ta-C (Tetrahedral Amorphous Carbon) Diamond Content (%) : ~ 85 Microhardnes HV/Gpa : 5000 / ~40 Thickness : 1.5 - 2µm Deposition Temperature : 80 degree celsius Coefficient of friction (Dry) : 0.