Technical Specification
Material
:
Ta-C (Tetrahedral Amorphous Carbon)
Diamond Content (%)
:
~ 85
Microhardnes HV/Gpa
:
5000 / ~40
Thickness
:
1.5 - 2µm
Deposition Temperature
:
80 degree celsius
Coefficient of friction (Dry)
:
0.